MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPR 3100 MT3 Polypropylene, Random Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Polypropylene PPR 3100 MT3 is a nucleated random copolymer polypropylene for the injection molding of articles with high transparency and excellent surface appearance.

Application

ATOFINA Polypropylene PPR 3100 MT3 is intended for general purpose, household goods, cosmetic caps and closures.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.525 g/cc0.0190 lb/in³ISO 1183
Density 0.902 g/cc0.0326 lb/in³ISO 1183
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8686ISO 2039-2
Tensile Strength, Yield 29.0 MPa4210 psiISO 527-2
Elongation at Yield 10 %10 %ISO 527-2
Tensile Modulus 1.30 GPa189 ksiISO 527-2
Flexural Modulus 1.20 GPa174 ksiISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 179
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 146 °C295 °FISO 3146
Vicat Softening Point 67.0 °C153 °F50N-50°C per hour; ISO 306
 130 °C266 °F10N-50°C per hour; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-22 ABS
LyondellBasell Moplen EP548Q Polypropylene, Impact Modified; Molded/Extruded
Formosa Plastics Formolene® 2710A Injection Molding RTPO Polypropylene
Formosa Plastics Formolene® 2510W Medium Impact Copolymer Polypropylene
Flint Hills PP 13T10A cs279 Random Copolymer Polypropylene

PFINAA108 / 38544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.