MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Neopolen® P 9235 0.035 g/cc Core density; Expanded Polypropylene (Europe)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Foamed

Material Notes: Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.

Physical properties of moldings made from Neopolen® P 9235.

Note: In order to measure the physical properties, parts with dimensions 300x200x60 mm were molded on a machine typical for the EPP industry under standard conditions. The properties can vary depending on part geometry and processing parameters.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0300 - 0.0360 g/cc0.00108 - 0.00130 lb/in³
Density 0.0350 g/cc0.00126 lb/in³ISO 845
Water Absorption <= 1.0 %
@Time 86400 sec
<= 1.0 %
@Time 24.0 hour
DIN 53428
Particle Size >= 1500 µm>= 1500 µm
 <= 4000 µm<= 4000 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.530 MPa76.9 psiDIN EN ISO 1798
Elongation at Break 34 %34 %DIN EN ISO 1798
Compressive Strength  0.150 MPa
@Strain 10 %
21.8 psi
@Strain 10 %
ISO 844
 0.180 MPa
@Strain 25 %
26.1 psi
@Strain 25 %
ISO 844
 0.280 MPa
@Strain 50 %
40.6 psi
@Strain 50 %
ISO 844
Compression Set 29 %
@Temperature 23.0 °C,
Time 79200 sec
29 %
@Temperature 73.4 °F,
Time 22.0 hour
50% RH; 24h after stress release; DIN EN ISO 1856 (Procedure C)
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0370 W/m-K0.257 BTU-in/hr-ft²-°FDIN 52612
Melting Point 120 - 180 °C248 - 356 °F
Decomposition Temperature >= 180 °C>= 356 °F
Flash Point >= 200 °C>= 392 °FASTM D1929
Ignition Temperature >= 360 °C>= 680 °FASTM D1929
 
Descriptive Properties
Average Particle Weight0.6 - 1.0 mg
ColorBlack
Commercial StatusEurope
Dimensional Stability at Heat<2%Linear size alterations after 4 d, 110°C; DIN ISO 2796

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe)
BASF Neopolen® P 8015 0.02 g/cc Core density; Expanded Polypropylene (Europe)
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe)
BASF Neopolen® P 9035 0.07 g/cc Core density; Expanded Polypropylene (Europe)

PBASG0045 / 131679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.