MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Cast, Metal Filled

Material Notes: Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ratios: A/B: 100/5.5 pbw (100/14.5 pbv); pot life: 5-8 hours; dark gray. Requires heat cure: 1-12 hours at 176-302° F (80-150° C). The Mastershop compounds are versatile, high-impact and wear resistant, and permanent. Good adhesion to metals, ceramics, glass, wood, fiberglass, masonry, and most rigid materials. Dimensionally stable and shrink-free. Almost unlimited shelf-life. Unaffected by atmospheric conditions, salt and fresh water, alkalis, diluted acids, many solvents, oils, and greases. Withstand temperatures up to 100° C (212° F) or 160° C for the “H” versions. Cured material is easy to machine with standard tools. Can be applied in any thickness. Ample working time.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0424 lb/in³Part B
 3.12 g/cc0.113 lb/in³Part A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83 - 8783 - 87
Tensile Strength at Break 3.45 - 41.4 MPa500 - 6000 psi
Flexural Strength 3.45 - 48.3 MPa500 - 7000 psi
Compressive Strength 62.1 - 89.6 MPa9000 - 13000 psi
Shear Strength 17.2 - 20.7 MPa2500 - 3000 psiAdhesive
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 - 720 min
@Temperature 80.0 - 150 °C
1.00 - 12.0 hour
@Temperature 176 - 302 °F
Pot Life 300 - 480 min300 - 480 min
 
Descriptive Properties
ColorDark Gray
Parts by Weight (pbw)100Part A
 5.5Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotchkote™ EG 503 Epoxy Metal Repair
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
3M Scotchkote™ SG 527 Epoxy Metal Repair
Overview of materials for Epoxy, Cast, Metal Filled
Polynt DISTITRON® VE 100 ST Epoxy Resin Based Vinyl Ester

PABC931 / 107915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.