MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ex-Tech Plastics PerformaTech™ PVC XSD-28 Static Dissipative PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Manufactured in thickness from 10 to 60 mils, PerformTech XSD-28 is available in rigid vinyl or PET. XSD-28 is a static dissipative sheet engineered specifically for ESD sensitive packaging for use in ESD controlled environments.

Characteristics:
Engineered for packaging to contain ESD-sensitive items and for use in ESD controlled environments.
Static Dissipative range 1 x 105 ohms per square to less than 1 x 1012 ohms per square.
Thickness ranging from .010 to .060”

End Uses:
Thermoformed containers.
High level of surface resistance and volume resistivity is ideal for the containment, transport and long-term storage of ICs, printed circuit boards and other ESD-sensitive components.

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 43.4 MPa6300 psiASTM D882
Elongation at Break >= 100 %>= 100 %ASTM D882
Izod Impact, Notched 1.44 J/cm2.70 ft-lb/inSOP-MEC-002.01
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+9 ohm1.00e+9 ohmEOS/ESD S11.11-1993
Surface Resistivity per Square 1.00e+10 ohm1.00e+10 ohm12% Humidity; ASTM D257
Static Decay <= 2.0 sec<= 2.0 secEIA 541
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 61.7 °C143 °FASTM D648-96
 
Descriptive Properties
12 day oven again4.7e10 OhmsASTM D257
Cold Impact-35°CASTM D1790
Contact Corrosivityno corrosionFTM 101C
Gauge Tolerance+/-5%gamma or beta gauges
Polycarbonate Compatibilityno attackEIA 564
Tribocharging<0.13 nC/in2Bellcore GR1421-CORE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Colorite Polymers CS9040UL--85B Non Lead Wire and Cable Vinyl Compound
Denka VINYKON S3098 PVC, S grade for refrigerator gaskets
CoreLite PVC 100 Closed-Cell PVC Foam Sheet
Arkema Lacovyl® S 071 S PVC
Arkema Nakan® FMM 871 N PVC, Soft Injection Molding Grade

PEXTEC993 / 133218

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.