MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyester (Thermoset) - Rigid
Categories: Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyester (Thermoset) - Rigid". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.601 - 2.20 g/cc0.0217 - 0.0795 lb/in³Average value: 1.76 g/cc Grade Count:50
Viscosity 110 - 180000 cP110 - 180000 cPAverage value: 14800 cP Grade Count:32
Linear Mold Shrinkage -0.00200 - 0.0350 cm/cm-0.00200 - 0.0350 in/inAverage value: 0.00216 cm/cm Grade Count:45
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5.00 - 68.05.00 - 68.0Average value: 36.3 Grade Count:39
Tensile Strength, Ultimate 10.0 - 123 MPa1450 - 17900 psiAverage value: 51.8 MPa Grade Count:53
Elongation at Break 0.500 - 2.40 %0.500 - 2.40 %Average value: 1.65 % Grade Count:6
Modulus of Elasticity 1.00 - 10.6 GPa145 - 1540 ksiAverage value: 4.03 GPa Grade Count:7
Flexural Yield Strength 53.8 - 265 MPa7800 - 38500 psiAverage value: 128 MPa Grade Count:49
Flexural Modulus 0.359 - 16.0 GPa52.0 - 2320 ksiAverage value: 10.2 GPa Grade Count:48
Compressive Yield Strength 71.0 - 214 MPa10300 - 31000 psiAverage value: 141 MPa Grade Count:46
Izod Impact, Notched 1.23 - 9.08 J/cm2.30 - 17.0 ft-lb/inAverage value: 4.08 J/cm Grade Count:36
Charpy Impact Unnotched 0.500 - 4.50 J/cm²2.38 - 21.4 ft-lb/in²Average value: 2.24 J/cm² Grade Count:10
Charpy Impact, Notched 0.300 - 4.50 J/cm²1.43 - 21.4 ft-lb/in²Average value: 2.21 J/cm² Grade Count:10
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+14 ohm-cm1.00e+12 - 1.00e+14 ohm-cmAverage value: 8.11e+13 ohm-cm Grade Count:10
Surface Resistance 1.00e+11 - 1.00e+13 ohm1.00e+11 - 1.00e+13 ohmAverage value: 8.11e+12 ohm Grade Count:10
Dielectric Constant 4.20 - 4.504.20 - 4.50Average value: 4.47 Grade Count:11
Dielectric Strength 10.8 - 30.0 kV/mm275 - 762 kV/inAverage value: 17.1 kV/mm Grade Count:46
Dielectric Loss Index 0.0300 - 0.04000.0300 - 0.0400Average value: 0.0310 Grade Count:10
Arc Resistance 143 - 220 sec143 - 220 secAverage value: 184 sec Grade Count:43
Comparative Tracking Index 500 - 600 V500 - 600 VAverage value: 526 V Grade Count:39
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.9 - 30.0 µm/m-°C6.60 - 16.7 µin/in-°FAverage value: 20.7 µm/m-°C Grade Count:11
Maximum Service Temperature, Air 71.0 - 200 °C160 - 392 °FAverage value: 121 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 50.0 - 140 °C122 - 284 °FAverage value: 85.5 °C Grade Count:22
Deflection Temperature at 1.8 MPa (264 psi) 200 - 260 °C392 - 500 °FAverage value: 252 °C Grade Count:46
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:46
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 138 - 171 °C280 - 340 °FAverage value: 153 °C Grade Count:35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyester Film
Overview of materials for Thermoset Polyester Glass Filled BMC
Overview of materials for Thermoset Polyester Glass SMC
Overview of materials for Epoxy Adhesive
Overview of materials for Phenolic; Unreinforced; Molded

O3500 / 78217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.