MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® 9012C Polyethylene HDPE, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: This high density polyethylene is an ethylene-hexene copolymer tailored for injection molded applications that require: • Good flow performance • Slip agent with good organoleptics and high oxidative stability • High impact strength • Excellent stiffness.

Typical injection molded applications for 9012C include items such as: • Caps • Closures • Containers.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D1505
ESCR 100% Igepal® 20 hour20 hourCondition B, F50; ASTM D1693
ESCR 10% Igepal® 13 hour13 hourCondition B, F50; ASTM D1693
Melt Flow 11.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Slip Level 1500 ppm1500 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 24.0 MPa3480 psi2 in/min, Type IV bar; ASTM D638
Elongation at Break 600 %600 %2 in/min, Type IV bar; ASTM D638
Flexural Modulus, 1% Secant 1170 MPa170000 psi16:1 span:depth, 0.5 in/min; ASTM D790
Izod Impact, Notched 0.450 J/cm
@Temperature 23.3 °C
0.843 ft-lb/in
@Temperature 74.0 °F
ASTM D256
Tangent Modulus 1250 MPa181000 psi16:1 span:depth, 0.5 in/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648, Method A
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C115 °FASTM D648, Method A
Vicat Softening Point 119 °C246 °FLoading 1, Rate A; ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FType A, Type I specimen; ASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Bamberger Polymers Bapolene® 3282 Injection Grade HDPE
Dow DOWLEX™ IP-10 High Density Polyethylene
LyondellBasell Alathon H 5057 High Denisty Polyethylene
Braskem HC7260LS-L HDPE Injection Molding Polyethylene

PCHEVC8908 / 241991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.