MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nitriflex Nitrilatex L-2108 Styrene Butadiene Latex
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: NITRILATEX synthetic lattices are divided into several groups, modified or not with carboxylic acid.

Applications: NITRILATEX synthetic lattices are specially indicated to impregnate cords, adhesives manufacture, fibers agglomeration, supported gloves manufacture, impregnation of non-woven, etc.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 38 - 41 %38 - 41 %Method L-001/P-065; ASTM D1417
pH 10.7 - 11.710.7 - 11.725°C, Method L-003; ASTM D1417
Brookfield Viscosity 43 cP43 cP(spindle=1, 20 rpm); ASTM D1417
Surface Tension 55 - 60 dynes/cm55 - 60 dynes/cmMethod L-005/L-040; ASTM D1417
 
Chemical PropertiesMetricEnglishComments
Styrene Content 21.5 - 25.5 %21.5 - 25.5 %ASTM D1417
 
Descriptive Properties
Coagulum Content %0-0.04ASTM D1417; Method L-004
Residual Styrene (ppm)0-0.1ASTM D1417, Method L-007

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nitriflex Nitrilatex NTL-350 Styrene Butadiene Latex
DuPont Mobility and Materials AquaStik® 2901 Latex
Master Bond LTX 119 Pressure Sensitive Acrylic Adhesive Latex Compound
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
DuPont Mobility and Materials AquaStik® AQS-1120 Polychloroprene Latex

PDAX067 / 29492

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.