MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese VECTRA® T130 30% Glass Filled Liquid Crystal Polymer (LCP)
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Description: A new 30% glass filled LCP with very high temperature capability and a UL V-0 rating at thin wall thicknesses required in today's E/E market.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ISO 1183
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ISO 2039-2
Tensile Strength at Break 140 MPa20300 psi5 mm/min; ISO 527-2/1A
Elongation at Break 1.5 %1.5 %5 mm/min; ISO 527-2/1A
Tensile Modulus 16.0 GPa2320 ksi1 mm/min; ISO 527-2/1A
Flexural Strength 210 MPa30500 psiISO 178
Flexural Modulus 15.4 GPa2230 ksiISO 178
Compressive Yield Strength 94.0 MPa13600 psiat 1% strain; ISO 604
Compressive Modulus 14.0 GPa2030 ksiISO 604
Izod Impact, Notched (ISO) 25.0 kJ/m²11.9 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²23.8 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 56.0 kV/mm1420 kV/inIEC 60243-1
Dissipation Factor 0.029
@Frequency 1e+6 Hz
0.029
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 V175 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 µm/m-°C
@Temperature 20.0 °C
1.67 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
CTE, linear, Transverse to Flow 19.0 µm/m-°C
@Temperature 20.0 °C
10.6 µin/in-°F
@Temperature 68.0 °F
ISO 11359-2
Melting Point 370 °C698 °FISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 300 °C572 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 244 °C471 °FISO 75-1, -2
Vicat Softening Point 226 °C439 °FISO 306
Flammability, UL94 V-0V-0thickness h
Oxygen Index 50 %50 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 355 - 365 °C671 - 689 °F
Middle Barrel Temperature 360 - 370 °C680 - 698 °F
Front Barrel Temperature 360 - 370 °C680 - 698 °F
Nozzle Temperature 355 - 365 °C671 - 689 °F
Melt Temperature 365 - 370 °C689 - 698 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Celanese VECTRA E135i LCP, 35% Glass Reinforced
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Stratasys® Ultem 9085 for Rapid Prototyping
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer

PHCW74 / 46015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.