MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Delrin® 150 Homopolymer Acetal (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the gap between metals and plastics. It possesses high tensile and flexural properties, along with creep resistance and toughness, while exhibiting low moisture absorption, and fatigue endurance.

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D792
Water Absorption 0.25 %
@Time 86400 sec
0.25 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.90 %0.90 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9494ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Tensile Modulus 3.10 GPa450 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.90 GPa420 ksiASTM D790
Compressive Strength 35.9 MPa5200 psiASTM D695
Izod Impact, Unnotched 0.80 J/cm1.5 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.200.2040 psi, 50 fpm; ASTM D3702
K (wear) Factor 111 x 10-8 mm³/N-M55.0 x 10-10 in³-min/ft-lb-hrASTM D3702
Limiting Pressure Velocity 0.0513 MPa-m/sec1460 psi-ft/minASTM D792
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 60 Hz
3.7
@Frequency 60 Hz
50% RH; ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.0050
@Frequency 60 Hz
0.0050
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 122 µm/m-°C68.0 µin/in-°FASTM D696
Melting Point 175 °C347 °FASTM D2133
Maximum Service Temperature, Air 85.0 °C185 °FContinuous; UL746B
 149 °C300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 169 °C336 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FASTM D648
Flammability, UL94 HBHBUL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 150 NC010 POM
Overview of materials for Acetal Copolymer, Unreinforced
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM)
Ensinger DELRIN® 507 Black Acetal Homopolymer (POM)
Overview of materials for Acetal Homopolymer, Unreinforced

PENSIN065 / 104756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.