MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled
Categories: Ceramic; Boride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Aremco’s refractory coatings offer the ultimate protection of high temperature components used in the processing of ceramics, glass, metals, and plastics.

Features

  • Ultra Hi-Temp Resistance
  • Non-Wetted by Molten Metals, Salts, Glass & Plastics
  • High Lubricity for Easy Part Release
  • Minimizes Cast Surface Defects
  • Increases Mold & Die Life
  • For Use in Oxidizing, Reducing & Vacuum Atmospheres
Applications:
  • Composite Forming
  • Glass Forming
  • Metal Casting
  • Injection Molding
  • Ceramic Hot-Pressing
  • Metal Powder Sintering
  • Welding
  • Brazing
Product Highlights: This patented coating is a two-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite crucibles, electrodes, and heat-treating fixtures to 2000°F (1093°C).

Key Words: High Temperature Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/cc
Solids Content 52.7 %52.7 %by volume
 79 %79 %by weight
pH 8.0 - 9.58.0 - 9.5coating
Viscosity 200 - 400 cP200 - 400 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 48.3 microns1.90 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1090 °C2000 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Cure Time >= 60.0 min>= 1.00 hourAir Set prior to curing
 15.0 min
@Temperature 760 °C
0.250 hour
@Temperature 1400 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorGray
Dry Film Coverage ft2/gal845at 1 mil
Mix Ratio by Weight60:40resin:hardener
Thinner623-T
Weight/Gallons12.5 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
H.C. Starck Grade F Titanium Diboride, TiB2
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
Ceradyne Ceralloy® 225 Titanium Diboride
3M Techical Ceramics Titanium Diboride
Goodfellow Titanium Diboride, TiB2

CAREM40 / 581

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.