MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Flexus® 7200 LLDPE Cast Film Extrusion  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing performance. Films obtained with this grade show excellent impact and puncture resistances. It contains antioxidant additives.

20µm film gauge, obtained in cast extruder

Applications: Stretch films; liners; LDPE and HDPE blends; packages for general use

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Thickness 20.0 microns0.787 mil
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 990 %990 %ASTM D882
Film Elongation at Break, TD 1040 %1040 %ASTM D882
Secant Modulus, MD 0.180 GPa26.1 ksi1%, Flexural; ASTM D882
Secant Modulus, TD 0.190 GPa27.6 ksi1%, Flexural; ASTM D882
Elmendorf Tear Strength, MD 12.5 g/micron318 g/milASTM 1922
Elmendorf Tear Strength, TD 23.0 g/micron584 g/milASTM 1922
Dart Drop 8.50 g/micron216 g/milF50; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 30.0 MPa4350 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 28 %28 %ASTM D1003
Gloss 60 %60 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Flexus® 9200 LLDPE Blown Film Extrusion
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade)
Borealis Borstar® FB2230 LLDPE for Film
Braskem Flexus® 7200 Cast Film Extrusion Polyethylene
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene

PBRAS111 / 27845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.