MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.

Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquids.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes...

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  20 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
20 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
 20 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
20 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
 20 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
20 cP
@Shear Rate 1000 1/s,
Temperature 572 °F
 120 cP
@Shear Rate 10 1/s,
Temperature 300 °C
120 cP
@Shear Rate 10 1/s,
Temperature 572 °F
 135 cP
@Shear Rate 100 1/s,
Temperature 300 °C
135 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 140 cP
@Shear Rate 100 1/s,
Temperature 290 °C
140 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 150 cP
@Shear Rate 100 1/s,
Temperature 280 °C
150 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 250 cP
@Shear Rate 10 1/s,
Temperature 290 °C
250 cP
@Shear Rate 10 1/s,
Temperature 554 °F
 300 cP
@Shear Rate 10 1/s,
Temperature 280 °C
300 cP
@Shear Rate 10 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.0062 cm/cm0.0062 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psiISO 527 Type 1A
Tensile Stress at Strain  30.0 MPa
@Strain 1 %,
Temperature 120 °C
4350 psi
@Strain 1 %,
Temperature 248 °F
 40.0 MPa
@Strain 1 %,
Temperature 80.0 °C
5800 psi
@Strain 1 %,
Temperature 176 °F
 80.0 MPa
@Strain 1 %,
Temperature -30.0 °C
11600 psi
@Strain 1 %,
Temperature -22.0 °F
 80.0 MPa
@Strain 1 %,
Temperature 0.000 °C
11600 psi
@Strain 1 %,
Temperature 32.0 °F
 80.0 MPa
@Strain 1 %,
Temperature 23.0 °C
11600 psi
@Strain 1 %,
Temperature 73.4 °F
 80.0 MPa
@Strain 3 %,
Temperature 120 °C
11600 psi
@Strain 3 %,
Temperature 248 °F
 100 MPa
@Strain 3 %,
Temperature 80.0 °C
14500 psi
@Strain 3 %,
Temperature 176 °F
 100 MPa
@Strain 6.0 %,
Temperature 120 °C
14500 psi
@Strain 6.0 %,
Temperature 248 °F
 120 MPa
@Strain 6.0 %,
Temperature 80.0 °C
17400 psi
@Strain 6.0 %,
Temperature 176 °F
 165 MPa
@Strain 2 %,
Temperature 0.000 °C
23900 psi
@Strain 2 %,
Temperature 32.0 °F
 165 MPa
@Strain 2 %,
Temperature 23.0 °C
23900 psi
@Strain 2 %,
Temperature 73.4 °F
 178 MPa
@Strain 2 %,
Temperature -30.0 °C
25800 psi
@Strain 2 %,
Temperature -22.0 °F
 190 MPa
@Strain 3 %,
Temperature 23.0 °C
27600 psi
@Strain 3 %,
Temperature 73.4 °F
 195 MPa
@Strain 3 %,
Temperature 0.000 °C
28300 psi
@Strain 3 %,
Temperature 32.0 °F
 215 MPa
@Strain 3 %,
Temperature -30.0 °C
31200 psi
@Strain 3 %,
Temperature -22.0 °F
Elongation at Break 3.0 %3.0 %ISO 527 Type 1A
Tensile Modulus 10.0 GPa1450 ksiISO 527 Type 1A
Flexural Strength 280 MPa40600 psiISO 178
 290 MPa42100 psiASTM D790
Flexural Modulus 9.00 GPa1310 ksiISO 178
 9.00 GPa1310 ksiASTM D790
Izod Impact, Notched 1.15 J/cm2.15 ft-lb/inASTM D256
Izod Impact, Unnotched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180/1eU
Charpy Impact Unnotched 8.00 J/cm²38.1 ft-lb/in²ISO 179/1eU
 4.20 J/cm²
@Temperature 135 °C,
Time 720000 sec
20.0 ft-lb/in²
@Temperature 275 °F,
Time 200 hour
ISO 179/1eU
 7.00 J/cm²
@Temperature 120 °C,
Time 720000 sec
33.3 ft-lb/in²
@Temperature 248 °F,
Time 200 hour
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 6.00e+14 ohm6.00e+14 ohmIEC 60093
Dielectric Constant 3.73.7IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
Dissipation Factor 0.0100.010IEC 60250
Comparative Tracking Index 500 V500 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
CTE, linear, Transverse to Flow 25.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F
@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/Af
 255 °C491 °FASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
Oxygen Index 23 %23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Dry
Domo TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY
Domo TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, DRY
Domo TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned

PRHOD637 / 137868

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.