MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccASTM D792-00
Water Absorption 0.30 %
@Temperature 22.8 °C,
Time 86400 sec
0.30 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570-98
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 62
@Time 15.0 sec
62
@Time 0.00417 hour
ASTM D2240-00
Tensile Strength 6.55 MPa950 psiASTM D412-98
Tensile Stress at Strain 6.55 MPa
@Strain 100 %
950 psi
@Strain 100 %
ASTM D412-98
Elongation at Break 420 %420 %ASTM D412-98
Tear Strength 21.0 kN/m120 pliASTM D1004-94
Compression Set 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-98 Method B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Brittleness Temperature -59.4 °C-75.0 °FASTM D746-98
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorTan

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing
Saint-Gobain Tygon® S3™ B-44-4X I.B. Pressure Tubing Formulation for filling, draining, transfer and processing applications
Saint-Gobain Norton® Tygon® 2075 Ultra Chemical Resistant Tubing Formulation

PSTGQ904 / 160400

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.