MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Global HI-830 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes:
  • High flow
  • Good stiffness

Applications:

  • Appliances
  • Electrical/Electronic applications
  • Household goods
  • Food packaging
  • Toys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 71
@Thickness 6.35 mm
71
@Thickness 0.250 in
ASTM D785
Tensile Strength, Yield 21.4 MPa3100 psiASTM D638
Flexural Yield Strength 41.4 MPa6000 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 1.57 J/cm
@Thickness 6.35 mm,
Temperature 22.8 °C
2.94 ft-lb/in
@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
@Thickness 6.35 mm
194 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 96.1 °C205 °FASTM D1525
Flammability, UL94  HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Descriptive Properties
AppearanceTransparent
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polyrex® PH-88 Polystyrene - High Impact
Versalis Edistir R 850E Polystyrene
INEOS Styrolution Polystyrol 158 K GR 2 PS
I. Stern LG-215 High Impact Polystyrene Extrusion Grade
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene

PGLOBX26 / 42180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.