MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 752 Nickel Silver 18%, Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.

Information provided by Eagle Brass Company

Key Words: UNS C75200, ASTM B122
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 70 - 7670 - 76Thickness > 0.020 Inch
Tensile Strength, Ultimate 538 - 627 MPa78000 - 91000 psi
Tensile Strength, Yield 517 - 621 MPa75000 - 90000 psi0.2% offset
Elongation at Break 3.0 - 7.0 %3.0 - 7.0 %in 2 in.
Tensile Modulus 124 GPa18000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000297 ohm-cm0.0000297 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 32.9 W/m-K228 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 65 %65 %
Nickel, Ni 18 %18 %
Zinc, Zn 17 %17 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alloy Wire International RW 45 Ni-Cu Resistance Wire
Constantan Thermocouple Wire
Cunife® Hard Magnetic Alloy
Ed Fagan EFI Alloy 79 Soft Magnetic Alloy
Overview of materials for Polyetheretherketone, Carbon Fiber Filled

NEAGLE205 / 147454

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.