MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI KYDEX® 2200LT Thermoplastic
Categories: Polymer; Thermoplastic

Material Notes: SMP800C compliant sheet for mass transit applications

KYDEX® 2200LT is a high performance thermoplastic sheet designed for use in mass transit interior applications where SMP800C or BSS7239 compliance is required.

KYDEX® 2200LT is a cost effective alternative to FRP that offers the additional benefit of weight savings. It meets the Federal Transit Administration (FTA) and the Federal Rail Administration (FRA) requirements for smoke emission and flammability as tested under ASTM E662 and ASTM E162. Additionally KYDEX® 2200LT meets the toxicity criteria defined by SMP800C and BSS7239.

Suggested Applications:

  • Seatbacks
  • Armrests
  • Window Shrouds
  • Bulkhead Components
  • Wall and Ceiling Panels

Features:

  • Meets flamespread and smoke development requirements listed in 49 CFR 238
  • Compliant to SMP800C and BSS7239 toxicity specifications
  • Excellent formability and fabrication characteristics
  • Allows for tight tolerance control
  • Excellent resistance to graffiti, chemicals, and staining

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength 52.7 MPa7640 psiASTM D638
Tensile Modulus 3.895 GPa564.9 ksiASTM D638
Flexural Strength 77.9 MPa11300 psiASTM D790
Flexural Modulus 3.11 GPa451 ksiASTM D790
Izod Impact, Notched 1.40 J/cm2.62 ft-lb/inASTM D256
Gardner Impact 40.9 J30.2 ft-lbASTM D5420
 14.2 J
@Temperature -129 °C
10.5 ft-lb
@Temperature -200 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 53.8 µm/m-°C29.9 µin/in-°FASTM D831
Deflection Temperature at 1.8 MPa (264 psi) 89.00 °C192.2 °FUnnannealed/Annealed; ASTM D658
 
Descriptive Properties
FlammabilityDS(1.5)<100)ASTM E662; Smoke Density
 DS(4.0)<200)ASTM E662; Smoke Density
 Is<35; No Burning DripASTM E162; Flame Spread Index
 PassSMP 800C; Bombardier Toxic Gas Generation
 PassBSS 7239; Boeing Toxic Gas Generation

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SEKISUI SPI KYDEX® FST2 Thermoplastic
SEKISUI SPI KYDEX® 430 ABS/PVC
SEKISUI SPI KYDEX® 410 ABS/PVC
SEKISUI SPI KYDEX® 110 Polymer Alloy Sheet
SEKISUI SPI KYDEX® 100 Polymer Alloy Sheet

PSEKIS035 / 185860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.