MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed Avalon® 9 PTFE, Graphite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Conductive Carbon Filled

Material Notes: Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 g/cc2.12 g/ccASTM D792
Deformation 8.0 %8.0 %2000 psi 78°F; ASTM D621
 14 %14 %1000 psi 300°F; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Yield 17.9 MPa2600 psiASTM D1457
Elongation at Break 225 %225 %ASTM D1457
Compressive Strength 23.4 MPa3400 psiASTM D695
Shear Strength  14.5 MPa
@Temperature 149 °C
2100 psi
@Temperature 300 °F
ASTM D732
 15.5 MPa
@Temperature 93.3 °C
2250 psi
@Temperature 200 °F
ASTM D732
 16.5 MPa
@Temperature 65.6 °C
2400 psi
@Temperature 150 °F
ASTM D732
 18.6 MPa
@Temperature 37.8 °C
2700 psi
@Temperature 100 °F
ASTM D732
 19.3 MPa
@Temperature 26.7 °C
2800 psi
@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.0700.07033.3 psi @ 150 fpm
Coefficient of Friction, Static 0.0500.05033.3 psi
K (wear) Factor 60.4 x 10-8 mm³/N-M30.0 x 10-10 in³-min/ft-lb-hr
 
Descriptive Properties
ColorDark Gray to Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled
Greene Tweed Avalon® 87 PTFE, Glass Filled
Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled
Greene Tweed Avalon® 56 PTFE
Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled

PGREEN60 / 42354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.