MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Finished product available as bar or wire.
Chicago Extruded Metal temper codes: H01, H02, H04

This alloy is registered with the U.S. EPA as Antimicrobial.

Information provided by Chicago Extruded Metals

Key Words: CDA 220, ASTM B36, ASTM B134, SAE J461, SAE J463
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 4242
Tensile Strength 276 - 621 MPa40000 - 90000 psi
Elongation at Break 3.0 - 50 %3.0 - 50 %
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000391 ohm-cm0.00000391 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 188.5 W/m-K1308 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 89 - 91 %89 - 91 %
Iron, Fe 0.050 %0.050 %
Lead, Pb 0.050 %0.050 %
Other, total 0.20 %0.20 %
Zinc, Zn 8.7 - 10.7 %8.7 - 10.7 %as balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chicago Extruded Metals BioBrass® UNS C26000 Copper-Zinc Alloy
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy
Chicago Extruded Metals BioBrass® UNS C22600 Copper-Zinc Alloy
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy
Overview of materials for Brass

NCHICA901 / 147620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.