MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6), DAM
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes:

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D792
Water Absorption 1.2 %1.2 %@ 24 hrs; ASTM D570
Water Absorption at Saturation 6.8 %6.8 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 93.1 MPa13500 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 5.86 GPa850 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 4.83 GPa701 ksiASTM D790
Compressive Strength 107 MPa15500 psiASTM D695
Shear Strength 66.9 MPa9700 psiASTM D732
Izod Impact, Notched 0.640 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C22.2 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
@Thickness 3.18 mm
415 °F
@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 3.18 mm
405 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 271 - 293 °C520 - 559 °F
Mold Temperature 93.3 - 121 °C200 - 250 °F
Drying Temperature 93.3 °C200 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Filler / ReinforcementGlass Bead
 Glass Fiber Reinforcement
FormsPellets
Generic MaterialNylon 6
Generic NamePolyamide 6 (Nylon 6)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® NY-20GF/10GB/000 Polyamide 6 (Nylon 6), Conditioned
Avient Edgetek® NY-20GF/000 FR Nylon 6, Glass Filled
RTP Company RTP PA6 20 GF BLK Nylon 6 (PA), Value Product - Glass Fiber - Heat Stabilized
Avient Edgetek® PC-10GF/000 FR Polycarbonate (PC), Glass Filled
Avient Edgetek® NL-20GF/000 BLACK Polyamide 612 (Nylon 612)

PH0POL0000 / 144569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.