MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
Categories: Metal; Ferrous Metal; Carbon Steel; Medium Carbon Steel

Material Notes: Description: SUPERELSO® 890 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 890 N/mm² (130 KSI), SUPERELSO® 890 enables to make weight savings or support higher stresses and thus carry higher payload. With a good quality of steel making process, an adapted chemical analysis (low alloying content) and an excellent precision in Industeel's fabrication process (thickness tolerance, uniform mechanical characteristics), SUPERELSO® 890 is easy to machine, to bend and to weld which simplify production and maintenance. By using S SUPERELSO® 890 and thus thinner plate in welded structures, you limit preheating conditions, you decrease quantity of consumables, welding time and so production costs.

Information provided by manufacturer.

Key Words: EE 890 TIIK4 according to NFA 36-204, S 890 QL according to EN 10137-2, S 890 Q, S 890 QL, S 890 QL1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 940 - 1100 MPa136000 - 160000 psiTypical
Tensile Strength, Yield >= 890 MPa
@Strain 0.2 %
>= 129000 psi
@Strain 0.2 %
Elongation at Break >= 11 %>= 11 %At 5%
 13 %13 %Typical At 5%
Charpy Impact  >= 30.0 J
@Temperature -20.0 °C
>= 22.1 ft-lb
@Temperature -4.00 °F
Transverse
 >= 40.0 J
@Temperature -20.0 °C
>= 29.5 ft-lb
@Temperature -4.00 °F
Longitudinal
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.040 - 0.070 %0.040 - 0.070 %
Carbon, C 0.18 %0.18 %
Chromium, Cr 0.80 %0.80 %
Copper, Cu 0.30 %0.30 %
Iron, Fe 93.91 - 93.94 %93.91 - 93.94 %As remainder
Manganese, Mn 1.5 %1.5 %
Molybdenum, Mo 0.60 %0.60 %
Nickel, Ni 2.0 %2.0 %
Phosphorus, P 0.025 %0.025 %
Silicon, Si 0.50 %0.50 %
Sulfur, S 0.015 %0.015 %
Vanadium, V 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures
ThyssenKrupp XABO® 960 Structural Steel
AISI 6118H Steel
ASTM A871 HSLA Steel Grade 60, Hot-Rolled, 5-35 mm (3/16 to 1 3/8 in.)
ThyssenKrupp XABO® 890 Structural Steel

NINDUST46 / 17584

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.