MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mid-Mountain Materials THERMOSEAL® 1000 Thermal Cement
Categories: Ceramic

Material Notes: Description: A family of high temperature resistant cements carefully formulated to withstand thermal expansion and contraction under fluctuating heat conditions. THERMOSEAL® THERMAL CEMENTS are excellent for use when placing gaskets and seals in wood and coal stoves, fireplaces and furnaces.

APPLICATION: Mix well before use. Apply with towel or by hand using rubber gloves. THERMOSEAL THERMAL CEMENTS are incombustible, nontoxic, and asbestos-free, and are easily cleaned up with warm water while wet. The high initial tack and viscosity hold the cement in place and prevents running, yet is low enough to allow good penetration into fibers and pores, thus creating excellent bonds on most surfaces.

PACKAGING:
  • 11 fl. oz. caulking tubes, 12 per case, approx. 13lbs/case
  • 32 fl. oz. caulking tubes, 9 per case, approx. 24 lbs/case
  • One gallon cans, 4 per case, approx. 34 lbs/case
  • Five gallon pail, 55 lbs/pail

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0476 lb/in³
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 538 °C1000 °FUse Limit
Softening Point 760 °C1400 °F
 
Descriptive Properties
Color, DryBlack
Color, WetBlack
Coverage70 LF32 oz cartridge
Cure TypeAir Setting
pHMildly Alkaline

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mid-Mountain Materials ARMATEX® SF22 Silicone Rubber Coated Glass Fabric
Mid-Mountain Materials THERMOSEAL® 2000 High Temperature Cement
Portland Cement with Treated Silica Fume
Mid-Mountain Materials ARMATEX® SF60 Silicone Rubber Coated Glass Fabric
BNZ Materials 375-L Insulating Cement

CMID58 / 1562

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.