MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow C758-80NA Polypropylene Impact Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes:
    Overview
  • Very easy mold filling and fast set up
  • Good balance of impact strength and stiffness
  • Contains a nucleating and antistatic additive
  • Complies with: U.S. FDA FCN 843, Canadian HPFB No Objection

DOW C758-80NA Polypropylene Resin is a nucleated, antistatic, very high flow, reactor grade polypropylene impact copolymer. It provides excellent processability, while maintaining a good balance of impact and stiffness. DOW C758-80NA Polypropylene Resin is intended for use injection molded automotive interior trim applications.

Former Dow grade acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Index of Compound 80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
80 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 25.7 MPa3730 psiASTM D638
Elongation at Yield 4.6 %4.6 %ASTM D638
Flexural Modulus, 1% Secant 1380 MPa200000 psiASTM D790A
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C223 °FUnannealed; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem C758-80NA Polypropylene Impact Copolymer
Overview of materials for Polypropylene Copolymer
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
ExxonMobil PP7085E1 Polypropylene Impact Copolymer
Eurotec® Tecolen® CP30 NL MY PPCP, impact modified, heat & UV stabilized, natural

PDOW0966 / 93302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.