MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NovaCentrix PChem Nano-silver printable conductors
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: PChem inks offer fast cure and low resistivity, leading to reduced material and processing costs with equivalent or superior performance. All ink formulations are water based, low VOC. Flexographic, screen-printable, and spray formulations are fully commercialized. Gravure, dispenser, letterpress, and offset formulations are in developmental stages awaiting the right business opportunity. Due to the unique stabilization mechanism used for our particles, we do not offer ink-jetable formulations.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.6651 - 1.108 g/cc0.02403 - 0.04005 lb/in³wet
Solids Content 40 - 68 %40 - 68 %
Filler Content 40 - 65 %40 - 65 %Silver (Ag)
Particle Size 0.020 µm0.020 µm
Viscosity 100 - 50000 cP100 - 50000 cP
Thickness 0.100 - 2.00 microns0.00394 - 0.0787 mil
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000050 - 0.000020 ohm-cm0.0000050 - 0.000020 ohm-cm
Surface Resistivity per Square 0.020 - 0.40 ohm0.020 - 0.40 ohm
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.00 - 95 %0.00 - 95 %
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0167 min0.000278 hour
 
Descriptive Properties
Adhesion5
Binder Systemno binders - cohesion by sintering
Conductive Filler TypeSilver (Ag)
Material TypeReady-To-Use Formulation
Recommended SubstratesMelinex 454, ST505, coated paper, others
Solvent Systemwater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silpuran® 6600/40 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3071/30 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3070/50 A/B Liquid Silicone Rubber
Wacker Elastosil® LR 3003/25 A/B Liquid Silicone Rubber
Overview of materials for Thermoset Polyurethane Foam, Unreinforced

PFLEXCM26 / 179428

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.