MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Apec® 2097 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (330°C/2.16kg) 8 cm³/10 min; high viscosity; easy release; UV stabilized; 'softening temperature (VST/B 120)=202 °C; injection molding - melt temperature 330 - 340°C; Lamp covers; Headlamp lenses

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
Melt Density 0.970 g/cc
@Temperature 330 °C
0.0350 lb/in³
@Temperature 626 °F
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/in60x60x2 mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/in60x60x2 mm; ISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 330 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 626 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 130 MPa18900 psiISO 2039-1
Tensile Strength, Yield 76.0 MPa11000 psi50 [mm/min]; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 [mm/min]; ISO 527-1/-2
Elongation at Yield 6.9 %6.9 %50 [mm/min]; ISO 527-1/-2
Tensile Modulus 2.45 GPa355 ksi1 [mm/min]; ISO 527-1/-2
Flexural Strength 110 MPa16000 psi2 [mm/min]; ISO 178
Flexural Modulus 2.45 GPa355 ksi2 [mm/min]; ISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 V100 VM; solution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 191 °C376 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 172 °C342 °FISO 75-1/-2
Vicat Softening Point 202 °C
@Load 5.10 kg
396 °F
@Load 11.2 lb
120°C/h; ISO 306
UL RTI, Electrical 150 °C302 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 150 °C302 °FUL 746B
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 25 %25 %Method A; ISO 4589-1/-2
Glow Wire Flammability Index 800 °C1470 °FIEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5061.506Procedure A; ISO 489
Transmission, Visible 89 %89 %1 mm; ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 330 °C626 °FInjection Molding; ISO 294
Mold Temperature 100 °C212 °FInjection Molding; ISO 10724
Injection Velocity 200 mm/sec7.87 in/secISO 294
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® LQ 2643 Polycarbonate, UV-Stabilized
Covestro Makrolon® LQ 2647 Polycarbonate, UV-Stabilized
Covestro Apec® 1695 Polycarbonate
SABIC Lexan® 133 PC
Delrin Delrin® 100 NC010 POM

PB09709 / 92549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.