MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos N20N-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: This is a high melt flow rate, nucleated polypropylene impact copolymer formulated for improved flowability. It has an optimum balance of stiffness and impact resistance for injection molded applications. This grade is vis broken and has antistat and a slip agent. It is particularly well suited for the Materials Handling industry in applications such as crates for food transport and storage. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.

    Applications
  • Materials handling products (crates)
  • Consumer products (pails, small containers)
  • Industrial applications

    Benefits
  • Medium to High impact resistance
  • Good impact to stiffness balance
  • Superior moldability

Information provided by Ineos Olefins & Polymers USA

Key Words: Optimum balance of stiffness and impact resistance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7474ASTM D785
Tensile Strength at Break 16.5 MPa2400 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 22.6 MPa3280 psi2.0 in/min; ASTM D638
Elongation at Break 50 %50 %2.0 in/min; ASTM D638
Elongation at Yield 5.0 %5.0 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1230 MPa179000 psiASTM D790A
Izod Impact, Notched 0.961 J/cm
@Temperature -20.0 °C
1.80 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Izod Impact, Notched (ISO)  9.30 kJ/m²
@Temperature -20.0 °C
4.43 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FUnannealed; ASTM D648
Vicat Softening Point 145 °C293 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 43 %43 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Instrumented Impact (Dynatup)Ductile23°C, D3763
 Ductilenegative 20°C, D3763
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ IP-10 High Density Polyethylene
Ineos H20Z-03 Polypropylene Homopolymer
Ineos N00M-00 Polypropylene Impact Copolymer
Ineos H20E-00 Polypropylene Homopolymer
ExxonMobil PP7654KNE2 Polypropylene Homopolymer

PINEOS060 / 99381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.