MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® BioClear
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Somos® BioClear produces clear, strong, tough and water-resistant parts. Developed for medical applications and is ISO 10993-5, ISO 10993-10 and USP VI certified.

Applications: Somos® BioClear is designed for medical applications that are non-implant and have limited contact with the body, such as dental drill guides and device prototyping.

Property data for UV-postcured material.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³
Water Absorption 0.35 %0.35 %ASTM D570-98
Viscosity 260 cP
@Temperature 30.0 °C
260 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 47.1 - 53.6 MPa6830 - 7770 psiASTM D638M
Elongation at Break 11 - 20 %11 - 20 %ASTM D638M
Elongation at Yield 3.0 %3.0 %ASTM D638M
Modulus of Elasticity 2.65 - 2.88 GPa384 - 418 ksiASTM D368M
Flexural Strength 63.1 - 74.2 MPa9150 - 10800 psiASTM D790M
Flexural Modulus 2.04 - 2.37 GPa296 - 344 ksiASTM D790M
Izod Impact, Notched 0.200 - 0.300 J/cm0.375 - 0.562 ft-lb/inASTM D256A
Graves Tear Strength 150 kN/m856 pliASTM D1004-09
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.4 - 3.5
@Frequency 1e+6 Hz
3.4 - 3.5
@Frequency 1e+6 Hz
ASTM D150-98
 3.7 - 3.9
@Frequency 1000 Hz
3.7 - 3.9
@Frequency 1000 Hz
ASTM D150-98
 3.9 - 4.1
@Frequency 60.0 Hz
3.9 - 4.1
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 15.4 - 16.3 kV/mm391 - 414 kV/inASTM D149-97A
 
Thermal PropertiesMetricEnglishComments
CTE, linear  60.0 - 67.0 µm/m-°C
@Temperature -40.0 - 0.000 °C
33.3 - 37.2 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-05
 90.0 - 96.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-05
 170 - 189 µm/m-°C
@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-05
 185 - 189 µm/m-°C
@Temperature 100 - 150 °C
103 - 105 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-05
Deflection Temperature at 0.46 MPa (66 psi) 45.9 - 54.5 °C115 - 130 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 49.7 °C120 - 121 °FASTM D648
Glass Transition Temp, Tg 39.0 - 46.0 °C102 - 115 °FASTM E1545-00
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.512 - 1.5151.512 - 1.515ASTM D542
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
AppearanceOptically clear
DP (mils)6.5Slope of cure-depth vs. ln (E) curve
E10 (mJ/cm2)54exposure that gives 0.254 mm (0.010 inch) thickness
Ec (mJ/cm2)11.5Critical Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2258 Polycarbonate
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
Elkem (Bluestar Silicones) SILBIONE® LSR 4301 Liquid Silicone Rubber
ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer

PDSM9884 / 161505

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.