MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carmel Olefins Capilene® SL 50 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: CAPILENE® SL 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade combines good stiffness and impact properties.

Applications: CAPILENE® SL 50 is suitable for injection molding of crates, battery cases and technical articles.

Information provided by Carmel Olefins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 27.0 MPa3920 psi50 mm/min; ASTM D638
Elongation at Yield 12 %12 %50 mm/min; ASTM D638
Flexural Modulus 1.25 GPa181 ksiASTM D790
Izod Impact, Notched  0.500 J/cm
@Temperature -20.0 °C
0.937 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 1.20 J/cm
@Temperature 23.0 °C
2.25 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
Vicat Softening Point 150 °C
@Load 1.02 kg
302 °F
@Load 2.25 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® EFE1068 NC010T PA66
Carmel Olefins Capilene® TR 50 Polypropylene Impact Copolymer
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, General Purpose
Carmel Olefins Capilene® TU 75 AV Polypropylene Impact Copolymer
Carmel Olefins Capilene® TT 75 AV Polypropylene Impact Copolymer

PCARM979 / 131154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.