MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitika elitel UE3320 Polyester, Flake
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Low molecular weight type UE3200, High OH type, Resin modifier, Resin raw material

UNITIKA elitel resins are thermoplastic saturated copolymeric polyester resins. Elitel resins are expanding their applications from products such as adhesives, paints, ink binders, and modifying agents to the products in new-generation high-tech fields.

Characteristics:

  • elitel products have superior adhesiveness and coatability. They exhibit excellent adhesiveness and coatability to films and molded products of plastic materials such as polyester, polyvinylchloride, polycarbonate, and cellulose acetate; steel materials such as steel plates; metal materials such as copper, and aluminum; woven or nonwoven fabrics from polyester and other fibers; papers, woods, and others.
  • elitel products may be hardened by combined use of a hardening agent.
  • Blending of an elitel resin with another elitel resin or a different resin provides alloys with more diversified resin properties. Additionally, elitel products are effective as a modifying resin for providing other resins with flexibility, coatability, toughness, and others.
  • elitel resins form films excellent in flexibility, electrical properties, weather resistance, as well in appearance and transparency: elitel resins retain consistent quality with smaller change in quality over time
  • They are also excellent hygienically.

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³JIS K-6911
Moisture Absorption at Equilibrium 0.30 %0.30 %60%RH
Viscosity 0.50 cP
@Temperature 200 °C
0.50 cP
@Temperature 392 °F
Melt
Viscosity Measurement 0.0800.080Limiting Viscosity
Molecular Weight 1800 g/mol1800 g/mol
 
Chemical PropertiesMetricEnglishComments
Acid Value 1.01.0[mgKOH/g}
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070
 
Thermal PropertiesMetricEnglishComments
Softening Point 63.0 °C145 °FJIS K-2531
Glass Transition Temp, Tg 40.0 °C104 °F
 
Descriptive Properties
AppearancePale yellow
Hydroxyl value60mgKOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unitika elitel UE3250 Polyester, Pellet
Unitika elitel UE3300 Polyester, Flake
Unitika elitel UE3240 Polyester, Pellet
Unitika elitel UE3230 Polyester, Flake
Unitika elitel UE3223 Polyester, Flake

PUNITIK933 / 177953

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.