MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SGL Carbon Group EK 3205 Carbon Graphite
Categories: Carbon; Graphite

Material Notes: Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.

Typical Applications: High Loaded Seals

Information provided by SGL Carbon Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.25 g/cc0.0813 lb/in³
Open Porosity <= 2.5 %<= 2.5 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115Size/Load - 5/100
Hardness, Shore C 102102
Modulus of Elasticity 30.3 GPa4400 ksi
Flexural Strength 114 MPa16500 psi
Compressive Strength 259 MPa37500 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.96 µm/m-°C
@Temperature 20.0 °C
2.20 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 20.8 W/m-K144 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 399 °C750 °FIn oxygen
Maximum Service Temperature, Inert 538 °C1000 °FReducing Atm.
 
Descriptive Properties
ImpregnationAntimony

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SGL Carbon Group EK 3245 Carbon Graphite
SGL Carbon Group EK 2240 Carbon Graphite
SGL Carbon Group EK 2200 Carbon Graphite
SGL Carbon Group EK 40 Graphite
SGL Carbon Group EI 2100 Carbon Graphite

ESGK09 / 5688

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.