MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borclean™ HC314BF Polypropylene Homopolymer for Capacitor Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Borclean HC314BF is a homopolymer film resin developed for use in the manufacture of the highest quality films for dielectric applications. Borclean HC314BF does not contain slip, antiblock, antistatic additives or nucleating additives.

Borclean HC314BF is especially suitable for biaxially oriented dielectrical film used in capacitors and manufactured on double bubble lines process for rough surface/impregnation capacitor film. It may also be used for metallisable film.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 3.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.9 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash 0.0010 - 0.0020 %0.0010 - 0.0020 %ISO 3451-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.252.25IEC 250
 
Thermal PropertiesMetricEnglishComments
Melting Point 161 - 165 °C322 - 329 °FISO 3146
 
Descriptive Properties
Calcium, ppm5from Anti-acid
Catalyst Residues, Aluminum ppm2 to 4
Catalyst Residues, Chloride ppm1 to 3
Catalyst Residues, Titanium ppm1 to 3
Isotactic Index %96Borealis

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borclean™ HC300BF Polypropylene Homopolymer for Capacitor Film
Borealis Borclean™ HB311BF Polypropylene Homopolymer for Capacitor Film
Borealis Borclean™ HC312BF Polypropylene Homopolymer for Capacitor Film
Borealis Borclean™ HC320BF Polypropylene Homopolymer for Capacitor Film
Borealis Borclean™ HC318BF Polypropylene Homopolymer for Capacitor Film

PBOREA036 / 27343

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.