MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay FM® 410-1 Core Splice Foam
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 410-1 adhesive foam is a modified epoxy adhesive foam designed for splicing honeycomb core under zero pressure, bonding of inserts or edge members to core and local honeycomb core reinforcement where increased shear strength is required. FM 410-1 adhesive foam contains no aluminum powder and has good radar transparency. FM 410-1 adhesive foam is supplied in sheet or roll form and may be cured in place with either free foaming or restrained foaming processes. The operating temperature is -67°F to 350°F (-55°C to 177°C).

Features & Benefits:

  • Improved handling characteristics
  • No metallic powders or asbestos
  • Splices honeycomb using ambient pressure
  • Bonds inserts or edge members to honeycomb core
  • Provides local honeycomb core reinforcement where increased shear is required
  • Cures in 60 minutes at 250°F to 350°F (121° to 177°C)
Applications:
  • Splicing honeycomb core
  • Bonding inserts or edge members to core
  • Localized reinforcement of honeycomb where increased shear strength is required

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.240 - 0.650 g/cc0.00867 - 0.0235 lb/in³
Volatiles <= 1.0 %<= 1.0 %
Storage Temperature <= -18.0 °C<= -0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  5.86 MPa
@Temperature 149 °C
850 psi
@Temperature 300 °F
Tube, 177°C Cure
 6.21 MPa
@Temperature 24.0 °C
900 psi
@Temperature 75.2 °F
Tube, 121°C Cure
 6.89 MPa
@Temperature 82.0 °C
1000 psi
@Temperature 180 °F
Tube, 121°C Cure
 6.89 MPa
@Temperature 82.0 °C
1000 psi
@Temperature 180 °F
Tube, 177°C Cure
 6.89 MPa
@Temperature -55.0 °C
1000 psi
@Temperature -67.0 °F
Tube, 121°C Cure
 7.58 MPa
@Temperature 24.0 °C
1100 psi
@Temperature 75.2 °F
Tube, 177°C Cure
 9.65 MPa
@Temperature -55.0 °C
1400 psi
@Temperature -67.0 °F
Tube, 177°C Cure
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBlue turning green during cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay FM® 73U Epoxy Film Adhesive
Solvay FM® 410 Adhesive Foam

PCYTED038 / 180340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.