MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD 6207 High Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: ExxonMobil™ HD 6207 is a homopolymer HDPE grade, characterized by high stiffness, high rigidity and high flow

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Thermal Stabilizer: Yes
Applications:
  • Drainage Pipes
  • Food packaging
  • Liquid Food Containers for Milk, Water and Juices

Information provided by ExxonMobil

Key Words: HDPE HYA 800
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ASTM D4883
ESCR 100% Igepal® <= 20.0 hour<= 20.0 hourF50; ASTM D1963
ESCR 10% Igepal® <= 20 hour<= 20 hourF50; ASTM D1963
Melt Flow  0.70 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 46 g/10 min
@Load 21.6 kg,
Temperature 190 °C
46 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64
@Time 15.0 sec
64
@Time 0.00417 hour
ASTM D2240
Tensile Strength, Yield 24.8 MPa3600 psi2 in/min; ASTM D638
Tensile Stress at Strain 13.8 MPa
@Strain 100 %
2000 psi
@Strain 100 %
2 in/min; ASTM D412
Elongation at Break >= 100 %>= 100 %2 in/min; ASTM D638
Tensile Modulus 1.38 GPa200 ksi2 in/min; ASTM D638
Izod Impact, Notched (ISO) 9.45 kJ/m²4.50 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 129 °C264 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 5404 High Density Polyethylene Resin
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade)
LyondellBasell Lupolen 3020 D LDPE
LyondellBasell Lupolen 3026 F LDPE, Film Grade
ExxonMobil LD 07523.AC Low Density Polyethylene Resin

PEX99327 / 175563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.