MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pau Tai UNINOX PA-551 PVC Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: UNINOX PA-551 is a high molecular weight acrylic polymer resin. This processing aid contributes greatly to rapid growth markets for rigid or flexible PVC compounds such as calendered sheet, extrusion profiles, blow molding and rigid foam extrusion.

Applications:

  • Pipe, particularly suited for high fillers content pipe
  • Pipe fittings
  • Calendered sheet
  • Extruded sheet and profiles
  • Injected-molded parts
  • PVC Foam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.220 - 0.420 g/cc0.00795 - 0.0152 lb/in³
Volatiles <= 1.0 %<= 1.0 %
Particle Mesh Size 35 Mesh35 Mesh2%
 
Descriptive Properties
AppearanceWhite Powder
Dosage, phr1.0-5.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pau Tai UNISTAB TM-381 Organo Tin Stabilizer
Pau Tai UNINOX AM-929 Acrylic Impact Modifier

PPAUTA130 / 56044

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.