MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Laprene® 8K1.A60 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Features adhesion on polar polymers

Laprene is a thermoplastic elastomer with SEBS. Applications include Automotive (soft skins, mats for glove compartments, keypads and soft-touch finishes, glass encapsulation), Building (extruded seals for doors and windows, simple and co-molded hydraulic seals), Household appliances (magnetic seals for refrigerators, power tools handles, remote controls covers, mobile phones covers, push-button panels, shock absorbing protections for vacuum cleaners), Sport and Leisure (items for diving such as flippers, snorkels, masks, and skiing such as ski pole handles, ski boots), Food (Synthetic corks for wine and liquor bottles, gaskets for food containers), Cosmetics (handles for toothbrushes and healthcare items, perfume bottle coatings)

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6161ASTM D 2240
Tensile Strength 12.0 MPa1740 psiASTM D412 C
Elongation at Break 550 %550 %ASTM D412-C
100% Modulus 2.10 MPa
@Strain 100 %
305 psi
@Strain 100 %
ASTM D412 C
Tear Strength 40.0 kN/m228 pliASTM D624 C
 
Descriptive Properties
AdhesionABS, PC, PC/ABS, PA6, PA6.6, PMMA, TPU, PBT, TPC, PS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Laprene® 8K1.A55 TPE
Celanese SO.F.TER Laprene® 8KS.A90/H TPE
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)
Kuraray SEPTON® S76 Soft Compound
Covestro Desmopan® 460 Thermoplastic Polyurethane

PSOFS727 / 162191

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.