MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes: Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 6.2 %6.2 %ISO 62
Moisture Absorption at Equilibrium 2.4 %2.4 %23°C/50% R.H.; ISO 62
Viscosity Number 150 cm³/g1.50 dl/g
Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 76.0 MPa11000 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 85.0 MPa12300 psi5mm/min; ISO 527
Elongation at Break 5.0 %5.0 %0.2 in/min; ASTM Test
 15 %15 %5mm/min; ISO 527
Tensile Modulus 4.60 GPa667 ksi1mm/min; ISO 527
 5.17 GPa750 ksiASTM Test
Flexural Modulus 4.00 GPa580 ksiISO Data
 4.10 GPa595 ksiASTM Test
Izod Impact, Notched 0.450 J/cm
@Temperature -40.0 °C
0.843 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 0.640 J/cm
@Thickness 3.17 mm
1.20 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 6.50 kJ/m²3.09 ft-lb/in²ISO Test
Charpy Impact Unnotched 22.0 J/cm²105 ft-lb/in²ISO 179
 14.5 J/cm²
@Temperature -30.0 °C
69.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor  0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
 0.020
@Frequency 100 Hz
0.020
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 450 V450 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
16.7 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 65.0 µm/m-°C36.1 µin/in-°FISO 11359
CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 195 °C383 °FASTM Test
 195 °C383 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °FASTM Test
 120 °C248 °FISO 75
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicHeat stabilized or stable to heat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® B3EG6 BK00564 30% Glass Filled PA6 (Dry)

PBASF9321 / 85085

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.