MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SAE 9254 Low Alloy Steel, Spheroidized Annealed and Cold Drawn Bar
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 9000 Series Steel; Low Alloy Steel

Key Words: UNS G92540
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³Typical Carbon Steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 187 - 241187 - 241
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Machinability 45 %45 %Cold Drawn AISI 1212 = 100%
Shear Modulus 78.0 GPa11300 ksiTypical Carbon Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.51 - 0.59 %0.51 - 0.59 %
Chromium, Cr 0.60 - 0.80 %0.60 - 0.80 %
Iron, Fe >= 96.14 %>= 96.14 %As Balance
Manganese, Mn 0.60 - 0.80 %0.60 - 0.80 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 1.2 - 1.6 %1.2 - 1.6 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 5160H Steel, normalized, 50 mm (2 in.) round
AISI 9260 Steel
AISI 9255 Steel, normalized at 900°C (1650°F)
AISI 5160H Steel, normalized, 25 mm (1 in.) round
AISI 9261 Steel (UNS G92610)

M9254 / 140328

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.