MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik COLORTREND® PLUS™ 802-7214 Universal Machine Colorant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Colortrend Plus 802 Colorants are environmentally friendly, no-VOC, AAPE-free universal colorants designed to have broad compatibility in trade-sales, water-based paints and solvent-based paints, as well as other products. The colorants comply with EPA Method 24 for having no volatile organic compounds. In addition, the colorants have been specially formulated to contain no alkyl phenol ethoxylates (APE).

Colortrend Plus 802 Machine Colorants are specially formulated for use in volumetric color dispensing machines for retail store and in-plant volumetric tinting. They are non-reactive with stainless steel and plastic materials used as components of dispensing machines. Aluminum, aluminum alloys and bi-metallic color machines should be avoided since they cause electrolytic corrosion or flocculation of the colorant.

Colortrend Plus 802 colorants remain in suspension with minimum agitation and do no skin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/cc
Solids Content 23.2 %23.2 %vehicle
 41.7 %41.7 %pigment
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Volatiles 35.1 %35.1 %volatiles include water
 
Descriptive Properties
ColorantPhthalo Blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO® Foamex 3062
Evonik TEGO® AddBond LTW-B Adhesion resin solution
Evonik SILIKOPHEN® AC 900 Methyl Polysiloxane Resin
Evonik CHROMA-CHEM® 844-1852 Industrial Colorant
Evonik CHROMA-CHEM® 844-1063 Industrial Colorant

PHUMB200 / 81202

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.