MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm PLEXIGLAS® Satinice df23 7N PMMA  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product Profile: PLEXIGLAS® Satinice df23 7N, based on PLEXIGLAS® 7N, is characterized by diffuse scattering of light. Typical properties of PLEXIGLAS® molding compound are
  • good flow
  • high mechanical strength, surface hardness and mar resistance
  • very good weather resistance.
Special properties of PLEXIGLAS® Satinice df23 7N are
  • excellent light diffusion combined with excellent light transmission.
Application: Used for injection molding items for lighting engineering applications

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Melt Flow 4.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
4.1 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psi5 mm/min; ISO 527
Elongation at Break 2.5 %2.5 %5 mm/min; ISO 527
Tensile Modulus 3.40 GPa493 ksiISO 527
Charpy Impact Unnotched 1.70 J/cm²8.09 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.180 J/cm²0.857 ft-lb/in²ISO 179/1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 113 µm/m-°C
@Temperature 0.000 - 50.0 °C
63.0 µin/in-°F
@Temperature 32.0 - 122 °F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 101 °C214 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75
Vicat Softening Point 105 °C221 °FB/50; ISO 306
Glass Transition Temp, Tg 108 °C226 °FISO 11357
Glow Wire Test 700 °C1290 °FIEC 60695-2
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 81 %81 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Die Temperature 220 - 260 °C428 - 500 °FExtrusion
Melt Temperature 220 - 260 °C428 - 500 °F
Drying Temperature <= 95.0 °C<= 203 °FPredrying
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourPredrying

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® 7N PMMA Molding Compound
Röhm Plexiglas® df21 8N Molding Compound
Röhm Plexiglas® df23 8N Molding Compound
Röhm PLEXIGLAS® Satinice df22 7N PMMA
Röhm Plexiglas® 8N PMMA Molding Compound

PEVONIL162 / 196366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.