MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Paint™ 634-AS-1 High Temperature Refractory Coating
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting by nonferrous molten metals, increasing the durability and erosion resistance of the underlying material. High dry film thicknesses from 10-50 mils can be achieved with this coating. Select 634-AS1 for high build applications.

Key Words: Coatings
Vendors: Aremco’s Pyro-Paint refractory coatings offer the ultimate protection of high temperature graphite, metal and refractory structures used in the processing of ceramics, glasses, metals, and plastics. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/cc
Solids Content 41 %41 %volume
 65 %65 %weight
pH 8.0 - 9.58.0 - 9.5Coating pH
Viscosity 10000 - 20000 cP10000 - 20000 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 63.5 microns2.50 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1260 °C2300 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Cure Time 120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorWhite
Coverage ft2/gal653Theoretical Coverage at 1 mil dry film thickness
Thinner634-AS1-T
Weight/Gallon12.5 lbs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
BASF Ultraform® N2320 006 POM
Polyplastics TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
Nabaltec ACTILOX® B60 AS1 AlO(OH) Boehmite
Nabaltec ACTILOX® 200 AS1 AlO(OH) Boehmite

CAREM57 / 598

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.