MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo PELPRENE™ P40H Polyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Features: Polyester TPE

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.48 %0.48 %23°C, 65% RH
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
Melt Index of Compound 10 g/10 min
@Temperature 190 °C
10 g/10 min
@Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989JIS K6301
Hardness, Shore D 3838ASTM D2240
Tensile Strength at Break 21.0 MPa3050 psiASTM D638
Elongation at Break 690 %690 %ASTM D638
50% Modulus 6.40 MPa
@Strain 50 %
6.40 MPa
@Strain 50 %
ASTM D638
Flexural Modulus 0.0510 GPa7.40 ksiASTM D790
Compressive Modulus 0.00450 GPa0.653 ksi10%; ASTM D695
Resilience 7878JIS K6301
Izod Impact, Notched NBNBASTM D256
Tear Strength 98.0 kN/m559 pliASTM D624
Taber Abrasion, mg/1000 Cycles 2020ASTM D1044
Compression Set 50 %50 %JIS K6301
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+12 ohm-cm2.00e+12 ohm-cmASTM D257
Dielectric Strength 20.0 kV/mm508 kV/inJIS K2111
 
Thermal PropertiesMetricEnglishComments
CTE, linear 170 µm/m-°C
@Temperature 20.0 °C
94.4 µin/in-°F
@Temperature 68.0 °F
TMA
Melting Point 172 °C342 °FBy DSC
Vicat Softening Point 120 °C248 °FASTM D1525
Brittleness Temperature <= -65.0 °C<= -85.0 °FJIS K6301
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Envalior Arnitel® EL250 TPC-ET
Sumitomo Chemical ESPOLEX® 907 Thermoplastic Elastomer
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)

PTOY666 / 70826

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.