System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Gichem GIPLENE DP08/TD Polypropylene
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 40% Talc Filler
Material Notes:
PP 40% talc, high dimensional and thermal stability, detergent stabilized. High injection speed.
Information provided by GICHEM Gruppo Industriale Chimico
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
g/cc
0.0452
lb/in³
ASTM D792
Water Absorption
0.020 %
0.020 %
ASTM D570
Linear Mold Shrinkage
0.0080
-
0.010
cm/cm
0.0080
-
0.010
in/in
ASTM D955
Melt Flow
10
g/10 min
10
g/10 min
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
28.0
MPa
4060
psi
ASTM D638
Elongation at Yield
3.0 %
3.0 %
ASTM D638
Flexural Modulus
4.00
GPa
580
ksi
ASTM D790
Izod Impact, Notched
0.250
J/cm
0.468
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
93.0
°C
199
°F
ASTM D648
Vicat Softening Point
106
°C
223
°F
ASTM D1525/A
Flammability, UL94
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Flammability Test
125
125
[°C] Bilia; IEC 331
Oxygen Index
21 %
21 %
ASTM D2863
Glow Wire Test
650
°C
1200
°F
IEC 695-2-1
Processing Properties
Metric
English
Comments
Middle Barrel Temperature
190
-
230
°C
374
-
446
°F
Mold Temperature
50.0
-
70.0
°C
122
-
158
°F
Drying Temperature
70.0
°C
158
°F
2 hours
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers
Borealis Bormed™ TD109CF Polypropylene Copolymer
Avient Lubri-Tech™ PP-20TC/8T-2S Polypropylene (PP), Talc Filled, PTFE/Silicone Lubricated
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer
Special Metals NIMONIC® Alloy 901
PGICH07 / 41824
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.