MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES HiFill® PP E GF40 CC 40% Glass Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight

Additive: Heat Stabilizer

Features: Chemically Coupled, Heat Stabilized and High Viscosity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength, Yield 89.6 MPa13000 psiASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Yield Strength 121 MPa17500 psiASTM D790
Flexural Modulus 7.58 GPa1100 ksiASTM D790
Izod Impact, Notched 1.17 J/cm
@Thickness 3.17 mm
2.20 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Strength 20.5 kV/mm520 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C15.0 µin/in-°FASTM D696
Melting Point 163 °C325 °F
Deflection Temperature at 0.46 MPa (66 psi) 163 °C325 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C310 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Pro® 4003 RC 40% Glass Filled Polypropylene
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled
Celanese Celstran® +PP-GF40-04CN15 PP, 40% Glass Reinforced
Celanese Celstran® PP-GF40-04 PP, 40% Glass Reinforced
Overview of materials for Polypropylene with 40% Glass Fiber Filler

PTPC0551 / 136489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.