MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® Extreme™ ETP-600S Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Faster cure rates
  • Improved flow at high shear rates
  • Slightly higher tensile strength
  • Improved resistance to compression set
  • Equivalent fluid and chemical resistance

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/ccUncompounded Viton
Mooney Viscosity 60
@Temperature 121 °C
60
@Temperature 250 °F
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 767616 hours Postcure; ASTM D2240
Tensile Strength at Break 18.3 MPa2650 psi16 hours Postcure; ASTM D412
Elongation at Break 225 %225 %16 hours Postcure; ASTM D412
50% Modulus 2.80 MPa
@Strain 50 %
2.80 MPa
@Strain 50 %
16 hours Postcure; ASTM D412
100% Modulus 7.90 MPa
@Strain 100 %
1150 psi
@Strain 100 %
16 hours Postcure; ASTM D412
Compression Set  34 %
@Temperature 150 °C,
Time 252000 sec
34 %
@Temperature 302 °F,
Time 70.0 hour
O-Rings, postcured; ASTM D395B
 50 %
@Temperature 150 °C,
Time 1.21e+6 sec
50 %
@Temperature 302 °F,
Time 336 hour
O-Rings, postcured; ASTM D395B
 51 %
@Temperature 200 °C,
Time 252000 sec
51 %
@Temperature 392 °F,
Time 70.0 hour
O-Rings, postcured; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -7.00 °C19.4 °FRetraction Temperature, Tr10; ASTM D1329
Glass Transition Temp, Tg -10.0 °C14.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature  177 °C
@Time 421 sec
351 °F
@Time 0.117 hour
Cure
 200 °C
@Time 57600 sec
392 °F
@Time 16.0 hour
Postcure
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 67 %67 %Uncompounded Viton
 
Descriptive Properties
Coloroff-white to tanUncompounded Viton
FormSheetUncompounded Viton
Formulation as Tested100ETP-600S
 3Luperox® 101-XL45
 3Diak 7 (TAIC)
 3Zinc Oxide
 30MT Black
OdorNoneUncompounded Viton
Storage StabilityExcellentUncompounded Viton

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® GBLT-600S Fluoroelastomer Compound
Chemours Viton® GF-600S Fluoroelastomer Compound
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
Chemours Viton® ETP-900 Fluoroelastomer (FKM)
Chemours Viton® B-70 Fluoroelastomer (FKM), Low Temperature Grade

PDVC9814 / 170455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.