MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GBC Grade 90 Alumina  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Data provided by the manufacturer, GBC Materials Corporation.

GBC Materials Corporation has been acquired by Morgan Advanced Ceramics.

Key Words: Al2O3, GBC Materials Corporation, aluminium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.64 g/cc0.132 lb/in³
Open Porosity 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Tensile Strength, Ultimate 180 MPa26100 psi
Flexural Strength 360 MPa52200 psi
Compressive Strength 1800 MPa261000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.00e+10 ohm-cm5.00e+10 ohm-cm
Dielectric Constant 8.18.1
Dissipation Factor 0.000400.00040
Dielectric Loss Index 0.00400.0040
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 µm/m-°C
@Temperature 20.0 °C
3.89 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1400 °C2550 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 90 %90 %
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
1035 Aluminum Composition Spec
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
GBC Grade 85 Alumina
3D Systems DuraForm® GF Glass Filled Nylon
Aluminum 6069-T4

CG0002 / 885

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.