Product Profile: ACRYLITE® Solar 0Z023 is an extruded acrylic sheet material (polymethyl methacrylate, PMMA) that is highly weather resistant and transparent. Special Properties: - UV transmission is specially adjusted to photovoltaic applications (PV, CPV),
- provides better energy conversion efficiency and module efficiency,
- longer service life of photo cells, lenses and covers
Other Typical Properties:- high mechanical strength, surface hardness and scratch resistance
- ease of processing
- good thermoformability
- high heat deflection temperature
- greater impact strength than glass combined with much lighter weight
Applications:- Covers for build-in photovoltaics
- Hot embossing of radial and linear Fresnel lenses for CPV/CSP applications
Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH. |