MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Henkel Loctite® Output™ 384 Thermally Conductive Repairable Acrylic Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Acrylic Bonding Adhesives and Thermally Conductive Bonders
Loctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond.

Loctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or microprocessors and their heat sinks. Loctite offers a wide range of adhesive chemistries including silicones, acrylics and epoxies. Many processing options are available for curing these adhesives such as heat cure, activator cure, and UV light.

Loctite® 384 1 component acrylic Output™ Thermally Conductive Repairable Acrylic Adhesive
Mounts components to heat sinks but allows removal for repair or replacement. Output™ Activator is required for curing. A repairable, room temperature curing adhesive used for parts subject to disassembly. Recommended Primer: Output™ Activator 20263. Cure Type: Activator 7387 Bonding Type: Acrylic Typical Use: Repairable adhesive for parts subject to disassembly

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
Viscosity 300000 - 800000 cP300000 - 800000 cPat 20 RPM
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 2.76 GPa400 ksi
Adhesive Bond Strength 5.17 MPa750 psiVaries with substrates
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C
@Temperature 20.0 °C
61.1 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.760 W/m-K5.27 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 50.0 °C122 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min0.0833 hourFixture time @ 20ºC
 240 - 1440 min4.00 - 24.0 hourFull Cure Time @ 20ºC
Shelf Life 9.00 Month9.00 Monthshelf life at 5ºC
 
Descriptive Properties
ColorWhite
Gap Fill0.01 in.
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 315 Acrylic Adhesive
Henkel Loctite® Output™ 383 Acrylic Adhesive
Henkel Loctite® 3151 1 component acrylic UV/Heat Cure Acrylic Adhesive
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive
Master Bond LTX 119 Pressure Sensitive Acrylic Adhesive Latex Compound

PLOCT167 / 51903

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.