MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Applied Silicone 40027 Liquid Silicone Rubber, 50 Durometer (LSR 50), Implant Grade
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes:

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/cc
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050Typical
 46 - 5546 - 55
Tensile Strength >= 6.55 MPa>= 950 psi
 6.89 MPa1000 psiTypical
Elongation at Break >= 350 %>= 350 %
 440 %440 %Typical
200% Modulus 3.55 MPa
@Strain 200 %
515 psi
@Strain 200 %
Tear Strength >= 28.0 kN/m>= 160 pli
 38.6 kN/m220 pliTypical
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 160 g/min160 g/minTypical
Cure Time 5.00 min
@Temperature 175 °C
0.0833 hour
@Temperature 347 °F
 
Descriptive Properties
Cure SystemPlatinum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) SILBIONE® LSR 4350 Liquid Silicone Rubber
Shin-Etsu Silicones LIMS™ KE1950-50A/B Elastomer
Overview of materials for Liquid Silicone Rubber
CHT Group QSil 218 Transparent, Liquid Silicone Rubber
BIW Liquid Silicone Rubber, Standard Grades

PNUSILA905 / 194574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.