MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Delrin Delrin® 100ST NC010 POM-HI
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Super Toughened High Viscosity Acetal Homopolymer

Information provided by DuPont; Delrin was sold by DuPont in 2023.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ISO 1183
Melt Density 1.14 g/cc
@Temperature 205 °C
0.0412 lb/in³
@Temperature 401 °F
Water Absorption 0.90 %
@Thickness 2.00 mm
0.90 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.350 %
@Thickness 2.00 mm
0.350 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4, 2577
Melt Flow  1.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.7 g/10 min
@Load 4.76 lb,
Temperature 374 °F
cm³/10min Volumetric; ISO 1133
 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5858ISO 2039-2
Hardness, Rockwell R 105105ISO 2039-2
Hardness, Shore D 707015s; ISO 48-4
Tensile Strength, Yield 41.0 MPa5950 psiISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Nominal; ISO 527-1/-2
Elongation at Yield 30 %30 %ISO 527-1/-2
Tensile Modulus 1.40 GPa203 ksiISO 527-1/-2
Flexural Strength 34.0 MPa
@Strain 3.5 %
4930 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 1.10 GPa160 ksiISO 178
Poissons Ratio 0.430.43
Izod Impact, Notched (ISO)  20.0 kJ/m²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 1100 MPa160000 psi1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 550 MPa79800 psi1000h; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 62631-3-2
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.4
@Frequency 100 Hz
4.4
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 140 µm/m-°C77.8 µin/in-°FISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Glass Transition Temp, Tg -35.0 °C-31.0 °F10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 41.0 mm/min
@Thickness 1.00 mm
1.61 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 °C392 °FOptimum, Extrusion
 195 - 205 °C383 - 401 °FRange, Extrusion
 200 - 210 °C392 - 410 °FRange, Injection
 205 °C401 °FOptimum, Injection
Mold Temperature 50.0 °C122 °FOptimum, Injection
 40.0 - 60.0 °C104 - 140 °FInjection
Drying Temperature 80.0 °C176 °FInjection
 80.0 °C176 °FExtrusion
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hourExtrusion, Dehumidified Dryer
 4.00 - 8.00 hour4.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.050 %<= 0.050 %Extrusion
 <= 0.050 %<= 0.050 %Injection
Hold Pressure 60.0 - 80.0 MPa8700 - 11600 psiInjection
 80.0 MPa11600 psiInjection
Annealing Temperature 160 °C320 °FOptional; 2 mm/min; Injection
 
Descriptive Properties
AdditivesRelease agent
Annealing time (min/mm)30Optional, Injection
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)6E-08
Emissions (mg/kg)<8VDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>POM-HI<ISO 11469
PolymerPOM
Processing Hold Pressure Time (s/mm)7.5Injection
Resin IdentificationPOM-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100ST BK602 POM-HI
Delrin Delrin® 500T NC010 POM-I
Delrin Delrin® 100STE NC010 POM-HI
Delrin Delrin® 500T BK602 POM-I
Delrin Delrin® 100 NC010 POM

PDSX5090 / 197730

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.