MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant® compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.51 g/cc1.51 g/ccASTM D792
Filler Content 30 %30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 177 MPa25700 psiType I, 51 mm/min; ASTM D638
Elongation at Break 9.0 %9.0 %Type I, 51 mm/min; ASTM D638
Flexural Strength 259 MPa37600 psiASTM D790
Flexural Modulus 8.96 GPa1300 ksiASTM D790
Izod Impact, Notched 1.20 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 360 - 382 °C680 - 720 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C
@Thickness 3.18 mm
>= 473 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 163 - 177 °C325 - 351 °F
Drying Temperature 104 °C219 °F
Dry Time 3.00 hour3.00 hour
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
AppearanceNatural Color
FeaturesBiocompatible
 Good Chemical Resistance
 Medium Impact Resistance
 Specialty Grade
FormsPellets
Generic MaterialPEEK
Generic NamePolyetheretherketone (PEEK)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesHigh Temperature Applications
 Hospital Goods
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK-CLASSIX™ (white) Life Science Grade
Greene Tweed Arlon® 2000 Polyketone
Lehvoss LUVOCOM® 1105-0904/GN2 PEEK with glass fiber
Mitsubishi Chemical Advanced Materials Ketron™ CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Westlake Plastics Lennite® GUR1050 (Type II) UHMW-PE For Medical Applications

PH0POL1251 / 145820

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.