MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Caprolactam Liquid
Categories: Fluid

Material Notes: Recommended use: Initial product for chemical syntheses, for the production of homopolymerisates and copolymerisates

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.014 g/cc
@Temperature 80.0 °C
0.03663 lb/in³
@Temperature 176 °F
 1.105 g/cc
@Temperature 20.0 °C
0.03992 lb/in³
@Temperature 68.0 °F
Relative
pH 7.0 - 8.57.0 - 8.5333 g/l
Viscosity 8.52 cP
@Temperature 80.0 °C
8.52 cP
@Temperature 176 °F
Dynamic
Molecular Weight 113.16 g/mol113.16 g/mol
Vapor Pressure  0.00000130 bar
@Temperature 20.0 °C
0.000975 torr
@Temperature 68.0 °F
 0.0000890 bar
@Temperature 60.0 °C
0.0668 torr
@Temperature 140 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 69.3 °C157 °FSolidification
Boiling Point 270.8 °C
@Pressure 0.1031 MPa
519.4 °F
@Pressure 14.96 psi
Flash Point >= 152 °C>= 306 °FDIN 51758
Ignition Temperature 365 °C689 °FDIN 51794
 
Descriptive Properties
Commercial StatusEurope
Solubility in Water866.89

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Vinyl Caprolactam
BASF Caprolactam Tablets

PBASG0213 / 131846

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.